Technology Process of Erbium nitride (ErN)
There total 8 articles about Erbium nitride (ErN) which
guide to synthetic route it.
The literature collected by LookChem mainly comes from the sharing of users and the free literature resources found by Internet computing technology. We keep the original model of the professional version of literature to make it easier and faster for users to retrieve and use. At the same time, we analyze and calculate the most feasible synthesis route with the highest yield for your reference as below:
synthetic route:
- Guidance literature:
-
In
neat (no solvent);
heating shavings of the metal with pure N2 at 1200°C;;
- Guidance literature:
-
With
pyrographite;
In
neat (no solvent);
heating in presence of 10 % Na2CO3 and C at 1250°C;;
- Guidance literature:
-
With
carbon;
In
neat (no solvent);
carbothermic reduction in N2 stream, powders of oxide and carbon mixed in mortar, heated (1500°C, 8 h); XRD;
DOI:10.1016/j.ssc.2011.07.021